Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 454N - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 454N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Styrolution® PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 14 cm³/10min ISO 1133
温度 200 °C -
荷重 5 kg -
溶融時の密度 935 kg/m³ -
溶融時の熱伝導率 0.165 W/(m K) -
溶融時の比熱 2290 J/(kg K) -
突き出し時の時の温度 81 °C -
機械的特性単位テスト基準
ISO データ
引張弾性率 2200 MPa ISO 527
降伏応力 27 MPa ISO 527
降伏ひずみ 1.4 % ISO 527
破壊呼びひずみ 25 % ISO 527
シャルピー衝撃強さ, +23°C 150 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 120 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 16 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 78 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 82 °C ISO 75-1/-2
ビカット軟化温度, B 82 °C ISO 306
線膨張係数, 平行 100 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.6 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 3.2 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 2.5 - IEC 62631-2-1
比誘電率, 1MHz 2.5 - IEC 62631-2-1
誘電正接, 100Hz 1.5 E-4 IEC 62631-2-1
誘電正接, 1MHz 4 E-4 IEC 62631-2-1
その他の特性.単位テスト基準
密度 1020 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 220 °C ISO 294
射出成形, 金型温度 40 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
機能
 粘度せん断速度. , Styrolution® PS 454N, PS-I, INEOS Styrolution
 せん断応力-せん断速度. , Styrolution® PS 454N, PS-I, INEOS Styrolution
 応力-ひずみ. , Styrolution® PS 454N, PS-I, INEOS Styrolution
 割線弾性率−ひずみ. , Styrolution® PS 454N, PS-I, INEOS Styrolution
 応力-ひずみ (等時的). 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 クリープ弾性率−時間. 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
クリープ曲線 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 応力-ひずみ (等時的). 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 クリープ弾性率−時間. 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
クリープ曲線 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 応力-ひずみ (等時的). 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 クリープ弾性率−時間. 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
クリープ曲線 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
 pvT , Styrolution® PS 454N, PS-I, INEOS Styrolution
 引張弾性率-温度. , Styrolution® PS 454N, PS-I, INEOS Styrolution
特殊な特性
成形加工法.
射出成形., フィルム押出成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良.
領域別の利用可能性
ヨーロッパ., 近東/アフリカ
その他の情報
村遜速揃
PROCESSING
injection molding, Melt temperature, range: 180 - 260 °C
injection molding, Melt temperature, recommended: 220 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 454N can be injection moulded under different conditions depending on machinery available and articles moulded. Mass temperature can be as high as 260°C. Polystyrol 454N is suitable for gas assisted injection moulding. To achieve articles with very high gloss well polished surfaces are recommended.
フィルム押出成形.
PROCESSING
Extrusion, Flat film, Melt temperature: 200 - 240 °C

Extrusion temperatures should not exceed 240°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.